Preparation and Durability Study of Anti corrosion Polyethylene Composite Materials
ZHANG Huan, LIU Hui
Preparation and Durability Study of Anti corrosion Polyethylene Composite Materials
External factors such as irradiation and light can cause the molecular chain of high density polyethylene(HDPE) to break and reduce its inherent properties. Therefore, improving the durability and corrosion resistance of HDPE is of great significance for expanding its application. In view of this situation, HDPE/m-CNT composites with high durability were prepared by using nitric acid modified carbon nanotubes (m-CNT) as fillers, and their mechanical properties and durability were studied. The results showed that the mechanical properties of HDPE/m-CNT composites were significantly increased due to the bridging effect of m-CNT on the matrix, and reached the maximum value in HDPE/m-CNT-3. In the photothermal durability, the tensile strength and compressive strength of HDPE/m-CNT-3 decreased by only 5.5% and 2.1% after 96 h aging, showing the best durability. Therefore, the above results show that the addition of m-CNT can effectively enhance the durability of HDPE composites.
1 |
张靖,郑成.高密度聚乙烯/氯磺化聚乙烯热塑性动态硫化弹性体的性能研究[J].橡胶工业,2023,70(11):857-861.
|
2 |
|
3 |
严善林,李秀英,刘燕.低密度聚乙烯/碳纤维复合材料的制备以及性能研究[J].塑料科技,2023,51(5):72-75.
|
4 |
盛旭敏.苎麻纤维/碳纤维/聚乙烯复合材料的性能研究[J].化工新型材料,2019,47(12):71-73, 78.
|
5 |
梁训美,于彦存,韩常玉,等.碳纤维增强中密度聚乙烯材料性能研究[J].塑料科技,2020,48(9):1-5.
|
6 |
|
7 |
|
8 |
|
9 |
|
10 |
|
11 |
|
12 |
|
13 |
|
14 |
|
15 |
|
16 |
|
17 |
|
18 |
|
19 |
|
20 |
|
21 |
|
22 |
|
23 |
|
24 |
|
25 |
|
26 |
|
27 |
|
28 |
|
29 |
|
/
〈 |
|
〉 |